In this study, to manufacture dental resin cement, Bis-GMA and HPMA were used as a major ingredient, camphoroquinone was used as a photoinitiator, TEGDMA was used as a diluent. And also, 2-isocyanato ethyl methacrylate was added to increase the bonding strength and 3-hydroxy pyridine was used as an additive for antibacterial property. The mixture made in accordance to the predetermined ratio was stirred for 24 hours and was polymerized at a wavelength of 440 to 480 nm for 40 seconds. It is considered that this material will be highly applicable as a dental resin cement with high quality. |
|